A、使用方法:將注塑機溫度調高 10 度至 20 度,把適量的清潔粉混合在塑料中(如轉用塑料,可混合將要使用的塑料),混合後將材料放入料斗中,先將馬達速度調慢,把混合料壓出 至模頭,待見到混合料後再把馬達速度調快少許,然後每隔 2 分鐘進行注塑。
B、用量:8安機:80-100 克清潔粉/2-4公斤塑料
24 安機:150-200克清潔粉/4-6公斤塑料
可先加入少許白礦油以防止清潔粉四散。因每種色粉及原料成份不同,以上份量亦按不同需要而定。
C、注意:如不慎把清潔粉沾入眼中,請用大量清水沖洗
A. Direction: Increase the injection molding machine temperature by 10 to 20℃ and blend the clean powder with the plastic then place them into funnel. Slow down the engine, launch the plastic with faster speed. Make the injection molding process every two minutes.
B. Usage: Injection molding machine (140T) :80-100g clean powder / 2-4kg plastic (Better to add white mineral oil to prevent the powder splash)
C. Caution: Keep away from children. If accidentally spray to eyes, rise with water and consult with the doctor immediately.